Armor 500T
Used For | Dimensions | Standards |
Armored | T: 3 - 80 mm | EN 10029 |
Mechanical Properties
Thickness(mm) | Hardness(HBW) | Charpy-V1) 10x10 mm test specimen2)Min. | Yield Strength Rp0.2(min MPa) | Tensile Strength Rm(MPa) | Elongation A5(min %) | Elongation A50(min %) |
3.0 - 80.0 | 480 - 540 | 32 J / -400C | 1250 | 1450 - 1750 | 8 | 10 |
Chemical Composition (ladle analysis)
C )(max %) | Si )(max %) | Mn )(max %) | P(max %) | S(max %) | Cr 1)(max %) | Ni 1)(max %) | Mo )(max %) | B )(max %) |
0.32 | 0.4 | 1.2 | 0.01 | 0.003 | 1 | 1.8 | 0.7 | 0.005 |
Tolerances
Thickness(mm) | Tolerances(mm) |
3.0 - 12.9 | - 0.0 / + 0.6 |
13.0 - 20.0 | - 0.0 / + 0.8 |
20.1 - 40.0 | - 0.0 / + 1.0 |
40.0 - 59.9 | - 0.0 / + 1.4 |
60.0 - 80.0 | - 0.0 / + 1.6 |
![]() |